Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 340 - 360 °C | 644 - 680 °F | Average value: 350 °C Grade Count:8 |
Overview of materials for PEKK, Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Melting Point | 262 - 360 °C | 504 - 680 °F | |
Indium Corp. Indalloy® 261 Bismuth-Silver Solder Alloy Information provided by the manufacturer, Indium Corporation of America. |
|||
Melting Point | 306 - 360 °C | 583 - 680 °F | Average value: 342 °C Grade Count:3 |
Overview of materials for PEKK, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate.. |