Material Notes:
Information provided by PTS LLC.
Physical Properties Metric English Comments
Specific Gravity 1.29 - 1.33 g/cc
1.29 - 1.33 g/cc
Dipping/distilled water; ISO 1183
Moisture Absorption at Equilibrium <= 0.3 %
<= 0.3 %
Loss on drying; ISO 15512
Viscosity Measurement 0.98 - 1.02
0.98 - 1.02
Intrinsic Viscosity, Phenol-tetrachloroethane; ISO 1628-5
Melt Flow 30 - 45 g/10 min

@Load 2.16 kg,
Temperature 250 °C
30 - 45 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
Ash <= 0.035 %
<= 0.035 %
Calcination; ISO 3451-1
Thermal Properties Metric English Comments
Melting Point 222 - 226 °C
432 - 439 °F
10°C/min; ISO11357 (DSC)
Descriptive Properties Value Comments
Carloxyl End Groups <30 mol/t
Phenol-chloroform dissolvent, Potentiometric titration
Color B <6.0
Pellet, C/2° light, Hunter Lab photometer