Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Quadrant Engineering Plastics Products
Trade Name Borotron®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very suitable for slowing down fast neutrons to lower energy thermal (slow) neutrons, which are then absorbed by the added boron compound. Whereas both PE-HMW and PE-UHMW are suitable for neutron shielding, PE-UHMW is often preferred because of its better deformation behaviour at high temperatures and its superior impact strength and wear resistance Effectively attenuates neutron radiation particles and minimises the gamma radiation released during their capture Very good wear and abrasion resistance High impact strength (particularly PE-UHMW) Excellent chemical resistance Low coefficient of friction Very low water absorption Moderate mechanical strength, stiffness and creep resistance Excellent machinability
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ISO 1183-1
Outgassing - Total Mass Loss 0.14 %
0.14 %
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Ball Indentation Hardness 55.0 MPa
7980 psi
ISO 2039-1
Tensile Strength 23.0 MPa
3340 psi
at Yield; ISO 527-1/-2
Elongation at Break 15 %
15 %
ISO 527-1/-2
Elongation at Yield 8.0 %
8.0 %
ISO 527-1/-2
Tensile Modulus 1.55 GPa
225 ksi
ISO 527-1/-2
Flexural Strength 28.0 MPa
4060 psi
Compressive Strength 13.5 MPa

@Strain 1 %
1960 psi

@Strain 1 %
ISO 604
20.5 MPa

@Strain 2 %
2970 psi

@Strain 2 %
ISO 604
28.5 MPa

@Strain 5 %
4130 psi

@Strain 5 %
ISO 604
K Factor (ISO) 150 µm/km
150 µm/km
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
ISO 179-1/1eU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
Complete Break; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.15 - 0.30
0.15 - 0.30
Sand Slurry 275
275
Limiting Pressure Velocity 0.0500 MPa-m/sec
1430 psi-ft/min
at 1 m/s unlubricated
0.0800 MPa-m/sec
2280 psi-ft/min
at 0.1 m/s unlubricated
Thermal Properties Metric English Comments
CTE, linear 140 µm/m-°C

@Temperature 23.0 - 100 °C
77.8 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.650 W/m-K
4.51 BTU-in/hr-ft²-°F
Melting Point 135 °C
275 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
Oxygen Index <= 20 %
<= 20 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+14 ohm-cm
>= 1.0e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+12 ohm
>= 1.0e+12 ohm
IEC 60093
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Continuous Sunlight Limited
Limited
Hot Water / Steam Unacceptable
Unacceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Limited
Limited
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Users viewing this material also viewed the following: