Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 1000 PE-UHMW, Black OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | DSC ISO 3146 |
Okulen® 1000 PE-UHMW, Conductive OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | DSC ISO 3146 |
Okulen® 1000 PE-UHMW, Green Black OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | DSC ISO 3146 |
Okulen® 1000 PE-UHMW, MoS2 -Moly- OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | DSC ISO 3146 |
Okulen® 1000 PE-UHMW, Multi-color OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, 588 Blue OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, 589 Blue OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, AB OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, DG OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, DryRun OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, F-Ex OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, GB OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, GB OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, L OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, Q OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, SG OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, SGB OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, SL OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, T OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, CL OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, OF OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, W OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 95.0 - 137 °C | 203 - 279 °F | |
Indium Corp. Indalloy 80 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 96.0 - 137 °C | 205 - 279 °F | |
Indium Corp. Indalloy 81 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | |
Addcomp PRIEX® Ionomer 48101 PP random copolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | |
Addcomp PRIEX® Ionomer 45101 PP random copolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |