Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 280 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 130 - 138 °C
266 - 280 °F
ISO 3146
Polikim ULPOLEN® 1000 UHMWPE Standard
Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia..
Melting Point 133 - 138 °C
271 - 280 °F
Polikim ULPOLEN® 1000 UHMWPE, UV, Antistatic
In tough operating conditions and under direct sunlight, standard Ulpolen® 1000 shows signs of wear and abrasion within a period shorter than a year. It accumulates static electric during daily use..
Melting Point 130 - 138 °C
266 - 280 °F
ISO 3146
Polikim ULPOLEN® 500 UHMWPE Standard
Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia..
Melting Point 133 - 138 °C
271 - 280 °F
Polikim ULPOLEN® 1000 UHMWPE, Oil
The solid lubricant additive reduces Ulpolen®'s coefficient of friction even further. As the additive is dry, it does not accumulate dust or dirt. In conveyor belts, it reduces squeakings at corner..
Melting Point 135 - 138 °C
275 - 280 °F
ASTM D789
Rochling Engineered Plastics Polystone® MPG Glass filled (UHMW-PE)
Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the ..
Melting Point 135 - 138 °C
275 - 280 °F
ASTM D789
Rochling Engineered Plastics Polystone® Natural (UHMW-PE)
Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the ..
Melting Point 135 - 138 °C
275 - 280 °F
ASTM D789
Rochling Engineered Plastics Polystone® XL Cross linked (UHMW-PE)
Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the ..
Melting Point 130 - 138 °C
266 - 280 °F
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Melting Point 130 - 138 °C
266 - 280 °F
Arkema Group KYNAR® 2751-00 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi..
Melting Point 56.7 - 138 °C
134 - 280 °F
Average value: 125 °C Grade Count:31
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..
Melting Point 130 - 138 °C
266 - 280 °F
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Melting Point 135 - 138 °C
275 - 280 °F
ASTM D789
Rochling Engineered Plastics Polystone® Reprocessed (UHMW-PE)
Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the ..
Copyright © lookpolymers.com All Rights Reserved