Thermal Properties Metric English Comments
Melting Point 1450 °C
2640 °F
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy
Inflection point 460°C. A nickel-iron controlled-expansion alloy containing 48% nickel. Its coefficient of thermal expansion is designed to match that of soft lead and soda-lime glasses. The a..
Melting Point 1450 °C
2640 °F
Special Metals NILO® Alloy K Controlled-Expansion Alloy
Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, mat..
Melting Point 1450 - 1480 °C
2640 - 2700 °F
Special Metals NI-SPAN-C® Alloy 902
A nickel-iron-chromium alloy made precipitation hardenable by additions of aluminum and titanium. The titanium content also helps provide a controllable thermoelastic coefficient, which is the allo..
Melting Point 1450 °C
2640 °F
Goodfellow Iron 58/Nickel 42 Alloy
Information provided by Goodfellow.
Melting Point 1450 °C
2640 °F
Goodfellow Nickel 70/Zirconium 30 Alloy
Information provided by Goodfellow.
Melting Point 1450 - 1510 °C
2650 - 2750 °F
Crucible Steel 420 and 420F Chromium Steel
Crucible 416 Plus is a hardenable chromium steel which is the general purpose cutlery grade. This grade is magnetic in all conditions. Information provided by Crucible Specialty Metals.
Melting Point 1450 °C
2642 °F
California Fine Wire Nickel 220 Super Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Melting Point 1450 °C
2642 °F
California Fine Wire Nickel 5900 Nickel Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Melting Point 1450 °C
2642 °F
California Fine Wire Nickel A 200 Nickel Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Melting Point 1450 °C
2642 °F
California Fine Wire Nickel Alloy 99
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Melting Point 1450 °C
2642 °F
California Fine Wire Nickel Alloy 99 Nickel Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Melting Point 1450 °C
2640 °F
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)
Data provided by Carpenter Technology Corporation.Kovar® alloy is a vacuum melted, Fe-Ni-Co, low expansion alloy whose chemical composition is controlled within narrow limits to assure precise unif..
Copyright © lookpolymers.com All Rights Reserved