Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 1480 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1450 - 1480 °C
2640 - 2700 °F
Special Metals NI-SPAN-C® Alloy 902
A nickel-iron-chromium alloy made precipitation hardenable by additions of aluminum and titanium. The titanium content also helps provide a controllable thermoelastic coefficient, which is the allo..
Melting Point 1370 - 1480 °C
2500 - 2700 °F
Crucible Steel 440C Chromium Steel
Crucible 440C is a hardenable chromium steel. It has one of the highest attainable hardnesses of the corrosion and heat resisting grades. This grade is magnetic at all times.Information provided b..
Melting Point 1430 - 1480 °C
2600 - 2700 °F
Crucible Steel 431 Chromium Steel
Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten..
Melting Point 1430 - 1480 °C
2600 - 2700 °F
Crucible Steel 431 Chromium Steel
Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten..
Copyright © lookpolymers.com All Rights Reserved