Material Notes:
Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, matches the expansion rate of borosilicate glasses and alumina ceramics. Used for glass-to-metal seals in applications requiring high reliability or resistance to thermal shock. Examples are high-power transmitting valves, transistor leads and headers, integrated-circuit lead frames, and photography flash bulbs. Standard product forms are round, tube, sheet, strip, and wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.16 g/cc
0.295 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 520 MPa
75400 psi
Annealed prior to test
400 MPa

@Temperature 300 °C
58000 psi

@Temperature 572 °F
Annealed prior to test
Tensile Strength, Yield 340 MPa

@Strain 0.200 %
49300 psi

@Strain 0.200 %
Annealed prior to test
140 MPa

@Strain 0.200 %,
Temperature 300 °C
20300 psi

@Strain 0.200 %,
Temperature 572 °F
Annealed prior to test
Elongation at Break 42 %
42 %
Annealed prior to test.
45 %

@Temperature 300 °C
45 %

@Temperature 572 °F
Annealed prior to test.
Thermal Properties Metric English Comments
CTE, linear 4.60 - 5.20 µm/m-°C

@Temperature 20.0 - 400 °C
2.56 - 2.89 µin/in-°F

@Temperature 68.0 - 752 °F
6.00 µm/m-°C

@Temperature 20.0 - 100 °C
3.33 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 16.7 W/m-K
116 BTU-in/hr-ft²-°F
Melting Point 1450 °C
2640 °F
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.10 %
<= 0.10 %
Carbon, C <= 0.040 %
<= 0.040 %
Chromium, Cr <= 0.20 %
<= 0.20 %
Cobalt, Co 17 %
17 %
Copper, Cu <= 0.20 %
<= 0.20 %
Iron, Fe 53 %
53 %
Magnesium, Mg <= 0.10 %
<= 0.10 %
Manganese, Mn <= 0.50 %
<= 0.50 %
Molybdenum, Mo <= 0.20 %
<= 0.20 %
Nickel, Ni 29 %
29 %
Silicon, Si <= 0.20 %
<= 0.20 %
Titanium, Ti <= 0.10 %
<= 0.10 %
Zirconium, Zr <= 0.10 %
<= 0.10 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000430 ohm-cm
0.0000430 ohm-cm