Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 8.91 g/cc
0.322 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 414 MPa
60000 psi
Annealed
793 MPa
115000 psi
Stress relieved
931 MPa
135000 psi
Hard
Tensile Strength, Yield 172 MPa
25000 psi
Annealed
552 MPa
80000 psi
Stress relieved
724 MPa
105000 psi
Hard
Modulus of Elasticity 204 GPa
29600 ksi
Thermal Properties Metric English Comments
CTE, linear 13.0 µm/m-°C

@Temperature 20.0 °C
7.22 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.456 J/g-°C

@Temperature 20.0 °C
0.109 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 61.6 W/m-K
428 BTU-in/hr-ft²-°F
Melting Point 1450 °C
2642 °F
Maximum Service Temperature, Air 1100 °C
2010 °F
Operating Temperature
Component Elements Properties Metric English Comments
Nickel, Ni 99 %
99 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000948 ohm-cm
0.00000948 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic Strong
Temperature Coefficient of Resistance 0.0048 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper -0.022