Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1450 °C | 2640 °F | |
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy Inflection point 460°C. A nickel-iron controlled-expansion alloy containing 48% nickel. Its coefficient of thermal expansion is designed to match that of soft lead and soda-lime glasses. The a.. |
|||
Melting Point | 1450 °C | 2640 °F | |
Special Metals NILO® Alloy K Controlled-Expansion Alloy Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, mat.. |
|||
Melting Point | 1450 - 1480 °C | 2640 - 2700 °F | |
Special Metals NI-SPAN-C® Alloy 902 A nickel-iron-chromium alloy made precipitation hardenable by additions of aluminum and titanium. The titanium content also helps provide a controllable thermoelastic coefficient, which is the allo.. |
|||
Melting Point | 1450 °C | 2640 °F | |
Goodfellow Iron 58/Nickel 42 Alloy Information provided by Goodfellow. |
|||
Melting Point | 1450 °C | 2640 °F | |
Goodfellow Nickel 70/Zirconium 30 Alloy Information provided by Goodfellow. |
|||
Melting Point | 1450 °C | 2640 °F | |
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy) Data provided by Carpenter Technology Corporation.Kovar® alloy is a vacuum melted, Fe-Ni-Co, low expansion alloy whose chemical composition is controlled within narrow limits to assure precise unif.. |