Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 345 MPa
50000 psi
Annealed
621 MPa
90000 psi
Stress relieved
758 MPa
110000 psi
Hard
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.544 J/g-°C

@Temperature 20.0 °C
0.130 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 185 W/m-K
1280 BTU-in/hr-ft²-°F
Melting Point 1450 °C
2642 °F
Maximum Service Temperature, Air 593 °C
1100 °F
Operating Temperature
Component Elements Properties Metric English Comments
Nickel, Ni 99.8 %
99.8 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000798 ohm-cm
0.00000798 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic Strong
Temperature Coefficient of Resistance 0.006 ohms/ohm-°C
0-100°C