Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

California Fine Wire NIFE 5200 Nickel Iron Resistance Wire

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Nickel Alloy
Manufacturer California Fine Wire
Trade Name NIFE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire NIFE 5200 Nickel Iron Resistance Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 8.44 g/cc
0.305 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 483 MPa
70000 psi
Annealed
827 MPa
120000 psi
Stress relieved
1030 MPa
150000 psi
Hard
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.523 J/g-°C

@Temperature 20.0 °C
0.125 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 28.9 W/m-K
201 BTU-in/hr-ft²-°F
Melting Point 1425 °C
2597 °F
Maximum Service Temperature, Air 1099 °C
2010 °F
Operating Temperature
Component Elements Properties Metric English Comments
Iron, Fe 30 %
30 %
Nickel, Ni 70 %
70 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000199 ohm-cm
0.0000199 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic Strong
Temperature Coefficient of Resistance 0.0052 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper -0.04