SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 148 MPa
21500 psi
5 mm/min; ISO 527
Elongation at Break 3.9 %
3.9 %
5 mm/min; ISO 527
Flexural Strength 211 MPa
30600 psi
2 mm/min; ISO 178
Flexural Modulus 7.00 GPa
1020 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.56
0.56
ASTM D3702 Modified
Coefficient of Friction, Static 0.48
0.48
ASTM D3702 Modified
K (wear) Factor 22.2 x 10-8 mm³/N-M
11.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
13.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 113 µm/m-°C

@Temperature 23.0 - 60.0 °C
62.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94