Polymer Property : Minimum Service Temperature, Air = -62.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Parker Chomerics CHO-BOND 360-208 Conductive Epoxy
Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting E..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Parker Chomerics CHO-BOND 584-208 Conductive Adhesive
Two-component, highly conductive adhesive system that combines the good adhesive characteristics of epoxy with the superior conductivity of silver. In addition to being available in bulk form, the m..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Parker Chomerics CHO-BOND 592 Conductive Epoxy
Highly conductive silver-filled epoxy adhesive which combines the best properties of metals and organics. This two-component system is unique in that it combines long pot life, good electrical condu..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Parker Chomerics CHO-BOND® 592 Conductive Adhesive
Description: CHO-BOND® 500 Series Adhesive/Sealant Compounds; These pure silver-filled materials are used where tight tolerances require thin bond lines. Various cure cycles are available, and the ..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Silicone Version
Parker Chomerics COMBO® and COMBO® Strip Gasketing Wire Mesh EMI Gasket Selection Guide
Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut GasketsAvailable Forms: Strips, Gaskets Made by Joining Strips.Standard Metals Available in EMI Portion: Monel ..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Silicone Version
Parker Chomerics Frame Gasketing Wire Mesh EMI Gasket Selection Guide
Construction: Formed Knitted Wire Strips Clamped in Aluminum ExtrusionsAvailable Forms: Strips, Fab. Lengths, Frames with Joined EMI Strips..Standard Metals Available in EMI Portion: Monel FerrexInf..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Silicone Version
Parker Chomerics PORCUPINE METALASTIC® Gasketing Wire Mesh EMI Gasket Selection Guide
Construction: Expanded Metal in ElastomerAvailable Forms: Sheets, Die-Cut GasketsStandard Metals Available in EMI Portion: Monel AluminumInformation provided by Chomerics
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Cured
Parker Chomerics Tecknit® 72-00008 Silver-Filled Epoxy System
Description: This commercial grade, conductive epoxy is designed for use in bonding applications where good conductivity is required. When mixed in a ratio of 1:1.4 by volume or weight, the two comp..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Cured
Parker Chomerics Tecknit® 72-08116 Silver-Filled Epoxy System
Description: This is a silver filled epoxy system designed for maximum performance and lowest volume resistivity. It is easily mixed 1:1 by volume or weight, from the two one-ounce jars. Its consist..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Parker Chomerics CHO-BOND 360-20 Conductive Epoxy
Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting E..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Silicone Version
Parker Chomerics COMBO® Gaskets Wire Mesh EMI Gasket Selection Guide
Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut GasketsAvailable Forms: Die-Cut Elastomer with Joined EMI Strips.Standard Metals Available in EMI Portion: Mone..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Silicone Version
Parker Chomerics MESH STRIP™ (Elastomer Core) Wire Mesh EMI Gasket Selection Guide
Construction: Knitted wire mesh over elastomer stripAvailable Forms: Strips, Gaskets Made by Joining Strips, Clip-On Strips.Standard Metals Available in EMI Portion: Monel Ferrex, Aluminum.Informati..
Minimum Service Temperature, Air -62.0 - -48.0 °C
-79.6 - -54.4 °F
Average value: -57.3 °C Grade Count:9
Overview of materials for Silicone, RTV, Construction Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Construction Grade". Each property range of values reported is minimum and maximum values..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Elasticity is retained to this temperature.
Momentive Performance Materials 1200® Construction Sealant
One-part, premium glazing sealant for structural as well as general purpose glazing. Cure Method: Acetoxy. Tack-free time
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Elasticity is retained to this temperature.
Momentive Performance Materials Contractors SCS 1000® Construction Sealant
One-part, for general purpose glazing and sealing applications. Cure Method: Acetoxy. Tack-free time
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Elasticity is retained to this temperature.
Momentive Performance Materials Sanitary 1700â„¢ Construction Sealant
One-part, mildew-resistant sealant for ceramic tile, showers, tubs, and plumbing fixtures. Cure Method: Acetoxy. Tack-free time
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Elasticity is retained to this temperature.
Momentive Performance Materials Ultraglaze® 4000 Construction Sealant
High strength, one-part structural glazing/weathersealing system. Cure Method: Alkoxy (Neutral). Tack-free time 2 to 5 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Sili..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Elasticity is retained to this temperature.
Momentive Performance Materials Ultraglaze® SSG 4000AC Construction Sealant
High strength, one-part, accelerated-cure structural glazing/weathersealing system.Cure Method: Alkoxy (Neutral). Tack-free time 1 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silico..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Elasticity is retained to this temperature.
Momentive Performance Materials Silglaze® II Construction Sealant
One-part, for channel, stop, and butt glazing. Primerless adhesion properties. Cure Method: Methoxy (Neutral). Tack-free time 0.5 hr. Peel Strength 30 lb/in.; Sag/slump 0.1 in.Data provided by ..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Tra-Con Tra-Bond 872-7TN1 Flexible Thixotropic Epoxy Adhesive
TRA-BOND 872-7TN1 is a flexible thixotropic epoxy. The high viscosity and long worklife make this material easy to handle. Also, the high thermal conductivity makes this product ideal for electronic..
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Dow Corning 735 OIL RESISTANT SEALANT
Black RTV that resists most oils, coolants, etc.Information provided by Dow Corning
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Dow Corning 738 ELECTRICAL SEALANT. WHITE
Durable general purpose sealant/adhesive for a wide variety of bonding and sealing applications. Can be used in applications where mil spec is required.Information provided by Dow Corning
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Silicone Version
Parker Chomerics POLASHEET® Metal EMI Gasket
Description: POLASHEET gasketing are composite EMI shielding and weather sealing materials. Either solid or sponge silicone may be specified as the weather seal. In POLASHEET gasketing individual mo..