Dow Corning 738 ELECTRICAL SEALANT. WHITE

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 738 ELECTRICAL SEALANT. WHITE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Durable general purpose sealant/adhesive for a wide variety of bonding and sealing applications. Can be used in applications where mil spec is required.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc

@Temperature 25.0 °C
1.03 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
Tensile Strength, Ultimate 2.65 MPa
385 psi
Elongation at Break 535 %
535 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Processing Properties Metric English Comments
Shelf Life 7.00 Month
7.00 Month
Descriptive Properties Value Comments
Color white
Flowable no