Polymer Property : Vicat Softening Point = 62.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 62.0 °C

@Load 1.00 kg
144 °F

@Load 2.20 lb
ISO 306/A
Polimeri Europa Greenflex® MH 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion
Greenflex MH 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Items produced with Greenflex MH 40 show high elasticity and good mechanical properties.Main Applic..
Vicat Softening Point 62.0 °C
144 °F
Rate B; ISO 306/B50
Premix Thermoplastics PRE-ELEC® PP 1395
PRE-ELEC PP 1395 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resist..
Vicat Softening Point 62.0 °C
144 °F
A<sub>50</sub> (10N); ASTM D1525 - ISO 306
DuPont Elvaloy® 1214 AC Ethylene and 14% Methyl Acrylate Copolymer  (discontinued **)
Elvaloy® 1214 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Vicat Softening Point 62.0 °C
144 °F
ASTM D1525
DuPont Bynel® 39E622 Adhesive Resin  (discontinued **)
Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Vicat Softening Point 62.0 - 124 °C
144 - 255 °F
Average value: 104 °C Grade Count:14
Overview of materials for Medium Density Polyethylene (MDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim..
Vicat Softening Point 62.0 - 131 °C
144 - 268 °F
Average value: 123 °C Grade Count:132
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Vicat Softening Point 62.0 °C
144 °F
ASTM D1525
DuPont™ Surlyn® 1855 Zinc Ionomer Resin for Blown and Cast Film  (discontinued **)
Surlyn® 1855 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Vicat Softening Point 62.0 °C
144 °F
LyondellBasell Lupolen® 3821 D MDPE
Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Vicat Softening Point 62.0 °C
144 °F
A; ISO 306
FKuR Kunststoff Bio-Flex® F 6611 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Vicat Softening Point 62.0 °C
144 °F
ASTM D1525
Mitsui ADMER® SF755A Elastomer Type Polyolefin
ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar..
Vicat Softening Point 62.0 °C
144 °F
ISO 306
Iran Petrochemical (PCC) MF3820 High Density Polyethylene
MF-3820 is a high molecular weight high density polyethylene. Application: bottle extrusion.Information provided by Iran Petrochemical Commercial Co.
Vicat Softening Point 62.0 °C
144 °F
ASTM D1525
SK Chemicals SKYTHANE® 850A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Vicat Softening Point 62.0 °C
144 °F
ASTM D1525
SK Chemicals SKYTHANE® S385A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Vicat Softening Point 62.0 °C
144 °F
ASTM D1525
SK Chemicals SKYTHANE® T850A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Vicat Softening Point 62.0 °C
144 °F
ASTM D1525
Lubrizol Estane® S385A Thermoplastic Polyurethane
Type: Estane® S385A is a Shore 85A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Information Provi..
Vicat Softening Point 62.0 °C
144 °F
ASTM D1525
Lubrizol Estane® S385AH Thermoplastic Polyurethane
Type: Estane® S385AH is a Shore 87A, polyester based thermoplastic polyurethane (TPU) with excellent transparency and Hydrolytic Stabilizer. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injectio..
Vicat Softening Point 62.0 °C
144 °F
ASTM D1525
DuPont Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin
Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Vicat Softening Point 62.0 °C
144 °F
Rate B, ASTM D1525-70
DuPont™ Surlyn® 9910 Ionomer Resin, Zinc
Surlyn® 9910 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Vicat Softening Point 62.0 °C
144 °F
Rate B, ASTM D1525-70
DuPont™ Surlyn® 7930 Ionomer Resin, Lithium
Surlyn® 7930 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne..
Vicat Softening Point 62.0 °C
144 °F
ASTM D1525
Arkema Group Orevac® 9307 Y Film EVA-MAH Terpolymer
EVA Terpolymers based Main Applications: Extrusion coating Skin packaging adhesive Thermo-adhesive filmsInformation provided by Arkema Group
Vicat Softening Point 62.0 °C

@Load 1.02 kg
144 °F

@Load 2.25 lb
ASTM-D1525
Braskem VA2019A EVA Foam Copolymer
The VA2019A is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium vinyl-acetate content. VA2019A is an easy processing product with high compatibility with other thermoplastic and elastomeric r..
Vicat Softening Point 62.0 °C
144 °F
50°C/hr; 50N
Arkema Group Evatane® 1020 VN 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for molding flexible articles. Examples: fittings, rail pads, medical.ISO data provided by the manufacturer, Arkema.
Vicat Softening Point 62.0 °C

@Load 0.999 kg
144 °F

@Load 2.20 lb
ASTM D1525
Arkema Group LOTADER® 4603 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4603 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure process in autoclave reactor. LOTADER 4603 is a multipurpose extrusion adhesive used..
Vicat Softening Point 62.0 °C

@Load 1.02 kg
144 °F

@Load 2.25 lb
ASTM-D1525
Braskem CN8092 EVA Molding Copolymer
CN8092 is an Ethylene-Vinyl Acetate copolymer (EVA) which has a molecular structure that provides easy processing, adhesion, resilience, low hardness, good moisture, and gas barrier properties. It i..
Vicat Softening Point 62.0 °C
144 °F
ASTM D1525
DuPont Bynel® 3859 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin  (discontinued **)
Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Vicat Softening Point 62.0 °C
144 °F
1000g; ASTM D-1525
ExxonMobil Escorene® LD-728 High EVA Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams..
Vicat Softening Point 62.0 °C
144 °F
ASTM D1525
SK Chemicals SKYTHANE® 385A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..