Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 62.0 °C @Load 1.00 kg |
144 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Greenflex® MH 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion Greenflex MH 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Items produced with Greenflex MH 40 show high elasticity and good mechanical properties.Main Applic.. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 1214 AC Ethylene and 14% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1214 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | ASTM D1525 |
DuPont Bynel® 39E622 Adhesive Resin
(discontinued **) Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 62.0 - 131 °C | 144 - 268 °F | Average value: 123 °C Grade Count:132 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | ASTM D1525 |
DuPont™ Surlyn® 1855 Zinc Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® 1855 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | |
LyondellBasell Lupolen® 3821 D MDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | A; ISO 306 |
FKuR Kunststoff Bio-Flex® F 6611 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | ASTM D1525 |
Mitsui ADMER® SF755A Elastomer Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | ISO 306 |
Iran Petrochemical (PCC) MF3820 High Density Polyethylene MF-3820 is a high molecular weight high density polyethylene. Application: bottle extrusion.Information provided by Iran Petrochemical Commercial Co. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | ASTM D1525 |
SK Chemicals SKYTHANE® T850A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | ASTM D1525 |
Lubrizol Estane® S385AH Thermoplastic Polyurethane Type: Estane® S385AH is a Shore 87A, polyester based thermoplastic polyurethane (TPU) with excellent transparency and Hydrolytic Stabilizer. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injectio.. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | ASTM D1525 |
DuPont Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Vicat Softening Point | 62.2 °C | 144 °F | ASTM D1525 |
ExxonMobil Escorene™ UL 00119 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00119 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic.. |
|||
Vicat Softening Point | 62.2 °C | 144 °F | ASTM D1525 |
ExxonMobil Escorene™ UL 00218CC3 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00218CC3 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperature above 240°C (464°F) may cause resin degradation.Availability: Africa & M.. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 9910 Ionomer Resin, Zinc Surlyn® 9910 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Vicat Softening Point | 62.2 °C | 144 °F | ASTM D1525 |
ExxonMobil Escorene® LD 720.01 Specialty Film Resin Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Vicat Softening Point | 62.2 °C | 144 °F | ASTM D1525 |
ExxonMobil Escorene® LD 720.62 Specialty Film Resin Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Vicat Softening Point | 62.2 °C | 144 °F | ASTM D1525 |
ExxonMobil Escorene® LD 721.IK Film Resin Escorene Ultra LD 721 is a high vinyl acetate copolymer specialty film resin providing outstanding heat sealability, along with excellent strength properties and clarity.Availability: Latin America,.. |
|||
Vicat Softening Point | 62.2 °C | 144 °F | ASTM D1525 |
ExxonMobil Escorene™ FL 00119 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00119 is a copolymer of ethylene and vinyl acetate offering low gel. Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Ap.. |
|||
Vicat Softening Point | 62.2 °C | 144 °F | ASTM D1525 |
ExxonMobil Escorene™ LD 706.15 Cast Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for coextruded cast film applications.Availability: Latin America, North America and South Ame.. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 7930 Ionomer Resin, Lithium Surlyn® 7930 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne.. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | ASTM D1525 |
Arkema Group Orevac® 9307 Y Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Skin packaging adhesive Thermo-adhesive filmsInformation provided by Arkema Group |
|||
Vicat Softening Point | 62.0 °C @Load 1.02 kg |
144 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem VA2019A EVA Foam Copolymer The VA2019A is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium vinyl-acetate content. VA2019A is an easy processing product with high compatibility with other thermoplastic and elastomeric r.. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1020 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for molding flexible articles. Examples: fittings, rail pads, medical.ISO data provided by the manufacturer, Arkema. |
|||
Vicat Softening Point | 62.0 °C @Load 0.999 kg |
144 °F @Load 2.20 lb |
ASTM D1525 |
Arkema Group LOTADER® 4603 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4603 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure process in autoclave reactor. LOTADER 4603 is a multipurpose extrusion adhesive used.. |
|||
Vicat Softening Point | 62.0 °C @Load 1.02 kg |
144 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem CN8092 EVA Molding Copolymer CN8092 is an Ethylene-Vinyl Acetate copolymer (EVA) which has a molecular structure that provides easy processing, adhesion, resilience, low hardness, good moisture, and gas barrier properties. It i.. |
|||
Vicat Softening Point | 62.2 °C | 144 °F | ASTM D1525 |
ExxonMobil Escorene™ FL 00218 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00218 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation. Machines should always b.. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | ASTM D1525 |
DuPont Bynel® 3859 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | 1000g; ASTM D-1525 |
ExxonMobil Escorene® LD-728 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |
|||
Vicat Softening Point | 62.0 °C | 144 °F | ASTM D1525 |
SK Chemicals SKYTHANE® 385A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |