Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) MF3820 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) MF3820 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MF-3820 is a high molecular weight high density polyethylene. Application: bottle extrusion.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.938 g/cc
0.0339 lb/in³
ISO 1183
Melt Flow 20 g/10 min

@Load 21.6 kg,
Temperature 190 °C
20 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ISO 527-1
Elongation at Yield 10 %
10 %
ISO 527-1
Tensile Modulus 0.650 GPa
94.3 ksi
ISO 527-1
Tensile Impact Strength 200 kJ/m²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
ISO 8256
Thermal Properties Metric English Comments
Vicat Softening Point 62.0 °C
144 °F
ISO 306
Heat Distortion Temperature 38.0 °C

@Pressure 1.80 MPa
100 °F

@Pressure 261 psi
ISO 57B-1
61.0 °C

@Pressure 0.450 MPa
142 °F

@Pressure 65.3 psi
ISO 75A-1