Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LD 516.LN Molding, Extrusion and Compounding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LD 516.LN Molding, Extrusion and Compounding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and uniform dispersion of additives. This resin can also be used in injection molding applications where it offers an outstanding balance of processability and end use performance.Availability: Latin America, North America and South AmericaAdditive: Antiblock: NoSlip: NoThermal Stabilizer: NoApplications: CapsClosuresCompoundingFood Packaging ContainersHouseware ArticlesInjection MoldingMasterbatch Base Resin Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ExxonMobil Method
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
15s; ASTM D2240
Hardness, Shore D 42
42
15s; ASTM D2240
Tensile Strength at Break 7.58 MPa
1100 psi
ASTM D638
Tensile Strength, Yield 11.0 MPa
1600 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Elongation at Yield 30 %
30 %
ASTM D638
1% Secant Modulus 234 MPa
34000 psi
ASTM D790
Impact Test 17.6 J
13.0 ft-lb
@ -4ºF, Instrumented Impact Total Energy; ASTM D3763
Thermal Properties Metric English Comments
Melting Point 110 °C
230 °F
Peak Melting Temperature; ExxonMobil Method
Vicat Softening Point 86.1 °C
187 °F
ASTM D1525
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved