Category Polymer , Film , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Film Grade
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Nucrel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Nucrel® 0908HS Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
9.2 wt% Methacrylic Acid.Nucrel® 0908HS is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and blown/cast film operations designed to process polyethylene resins.Typical Applications: Foil-containing shampoo, toothpaste, towelette, condiment and miscellaneous non-food pouches and sachets; Snack structures; Other foil, metallized film, or paper coatings as a heat seal or tie layer.Features & Benefits: Excellent adhesion to unprimed foil, paper and metallized film provides substrate protection for improved structure reliability and barrier integrity. Very good adhesion to low density polyethylene. Enhanced thermal stability for better extrusion and purging, improved extrusion web stability, and reduced gel formation. High drawability for high speed, thin gauge coating applications. Low seal initiation temperature allows for high speed packaging. Good hot tack, sealability through contamination and heat seal strength provide strong, reliable heat seals.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 84.0 °C
183 °F
Freezing Point via DSC/ASTM D3418
103 °C
217 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Processing Properties Metric English Comments
Nozzle Temperature 285 °C
545 °F
Typical Die Temp.
Melt Temperature 250 - 305 °C
482 - 581 °F