Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 7250 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 50.0 MPa

@Temperature 23.0 °C
7250 psi

@Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Crastin® ST820 BK503 PBT  (Unverified Data**)
Crastin® ST820 BK503 is an unreinforced, Super Tough, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Flexural Strength 50.0 MPa

@Temperature 275 °C
7250 psi

@Temperature 527 °F
ISO 178
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
Flexural Strength 50.0 MPa

@Temperature 225 °C
7250 psi

@Temperature 437 °F
Result based on 450GL30; ISO 178
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
Flexural Strength 50.0 MPa

@Strain 8.00 %
7250 psi

@Strain 8.00 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® A 30 S H3.0 000000 Nylon 66, Injection Molding
PA 66, non-reinforced, injection moldingInformation provided by LANXESS.
Flexural Strength 50.0 MPa

@Strain 6.00 %
7250 psi

@Strain 6.00 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Flexural Strength 50.0 MPa

@Strain 8.00 %
7250 psi

@Strain 8.00 %
Conditioned; ISO 178
Lanxess Durethan® A 30 H3.0 000000 Nylon 66
PA 66, non reinforced, injection molding, heat-ageing stabilized
Flexural Strength 50.0 MPa

@Temperature 80.0 °C
7250 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 50.0 MPa

@Temperature 80.0 °C
7250 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® NB-5550 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 50.0 MPa

@Temperature -40.0 °C
7250 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-222SA Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 50.0 MPa

@Temperature 80.0 °C
7250 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-422VOR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 50.0 MPa

@Temperature 23.0 °C
7250 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 3.5%); ASTM-D790
Toyobo GLAMIDE® T-802 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 50.0 MPa

@Treatment Temp. 200 °C,
Time 3600 sec
7250 psi

@Treatment Temp. 392 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m..
Copyright © lookpolymers.com All Rights Reserved