Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 105 - 157 kN/m | 599 - 896 pli | ASTM D624-95 |
Multibase Multi-Flex® TPO D 5302 E BLK Data provided by Multibase. |
|||
Tear Strength | 105 kN/m | 599 pli | Die C; ASTM D-624-95 |
Multibase Multi-Flex® TPO D-6403 Multi-Flex® D 6403 is a rubber modified polypropylene compound for automotive applications such as bumper-covers, step in pads, rubstrips, and airdams.Data provided by Multibase. |
|||
Tear Strength | 105 kN/m | 599 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible B6DT0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM D624-95 |
Multibase Multi-Flex® TPO D-6206 This TPO product was developed for facia applications exhibiting adhesion for current automotive paint systems.Data provided by Multibase. |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 6 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 105 kN/m | 599 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible B6DB1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 105 kN/m | 599 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible C5D01 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 105 kN/m | 599 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible G92B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 105 kN/m | 599 pli | ISO 34B |
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling .. |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM D624 |
Huntsman IROGRAN® A 95 K 4640 TPU-For Seals Introduction: IROGRAN A95K 4640 is a caprolactone-based thermoplastic polyurethane. The material has been developed for injection molding applications requiring exceptional performance in terms of c.. |
|||
Tear Strength | 105 kN/m | 599 pli | ISO 34B |
Huntsman AVALON® 85 AB Thermoplastic Polyurethane Introduction: AVALON 85 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Tear Strength | 105 kN/m | 599 pli | ISO 34B |
Huntsman AVALON® 90 AE Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
Tear Strength | 105 kN/m | 599 pli | DIN 53515 |
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 6 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 105 kN/m | 599 pli | Die C; ASTM D624 |
Lubrizol Estane® 2102-80A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Tear Strength | 105 kN/m | 599 pli | Die C; ASTM D624 |
Lubrizol Estane® 2103-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Tear Strength | 105 kN/m | 599 pli | Die C; ASTM D624 |
Lubrizol Estane® 2103-84AEN Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Contains UV Stabilizer, NSF Standard 61 certifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pelletha.. |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM D624 |
Lubrizol Estane® 2355-95AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Fuel resistant, extrusion laminate coatingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Dow Chemical.Lubrizol acquired the Pellethane.. |
|||
Tear Strength | 105 kN/m | 599 pli | Die C; ASTM D624 |
Lubrizol Estane® 2355-95AEF Thermoplastic Polyurethane Type: Pellethane® 2355-95AEF is a thermoplastic polyurethane elastomer.Feature: Film resin, Fuel resistant, Blow molding grade resin.Information Provided by The Lubrizol Corporation |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM D624 |
ELASTO UK Dryflex® 420501S SBS Based Material, 50D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM D624 |
ELASTO UK Dryflex® 422501S SBS Based Material, 50D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 105 kN/m | 599 pli | Die C; ASTM D624 |
Covestro Bayflex® 180 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR2202-95A Seal Grade TPU Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tear Strength | >= 105 kN/m | >= 599 pli | ISO 34 |
Austin Novel Materials Texalan® 590A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tear Strength | 105 kN/m | 599 pli | Parallel to flow; ISO 34-B |
AlphaGary Evoprene™ LF 6158 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Tear Strength | >= 105 kN/m | >= 599 pli | ISO 34 |
Austin Novel Materials Texalan® 395A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM D624 |
BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Tear Strength | 105 kN/m | 599 pli | Die C; ASTM D624 |
Lubrizol Pellethane® 2363-55DE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Tear Strength | 105 kN/m | 599 pli | Nicked; ISO 34-1B |
Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane Type: Estane® GP 52DT is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |
|||
Tear Strength | 105 kN/m | 599 pli | ISO 34B |
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane Introduction: AVALON 85 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABU is part of the AVALON Perform Range and offers a premi.. |