Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPO D-6206

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO D-6206.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This TPO product was developed for facia applications exhibiting adhesion for current automotive paint systems.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792-91
Melt Flow 6.0 g/10 min
6.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 17.2 MPa
2490 psi
ASTM D638-95
Elongation at Break 475 %
475 %
ASTM D638-95
Flexural Strength 20.7 MPa
3000 psi
ASTM D790-95
Flexural Modulus 1.0345 GPa
150.04 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched NB
NB
ASTM D-256-93a
Gardner Impact NB
NB
ASTM D-5420-93
Tear Strength 105 kN/m
599 pli
ASTM D624-95
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved