Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0123 cm/cm
0.0123 in/in
ASTM D955-89
Melt Flow 1.2 g/10 min
1.2 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 19.3 - 28.3 MPa
2800 - 4100 psi
ASTM D638-95
Elongation at Break 400 - 900 %
400 - 900 %
ASTM D638-95
Flexural Modulus 0.609 - 0.859 GPa
88.3 - 125 ksi
Secant 1%; ASTM D-790-95
Tear Strength 105 - 157 kN/m
599 - 896 pli
ASTM D624-95