Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 105 - 157 kN/m | 599 - 896 pli | ASTM D624-95 |
Multibase Multi-Flex® TPO D 5302 E BLK Data provided by Multibase. |
|||
Tear Strength | 105 kN/m | 599 pli | Die C; ASTM D-624-95 |
Multibase Multi-Flex® TPO D-6403 Multi-Flex® D 6403 is a rubber modified polypropylene compound for automotive applications such as bumper-covers, step in pads, rubstrips, and airdams.Data provided by Multibase. |
|||
Tear Strength | 105 kN/m | 600 pli | Die C; ASTM D624 |
Northstar Polymers MSS-A90A High Performance Polyurethane Cast Elastomer System 90A This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio.. |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM D624-95 |
Multibase Multi-Flex® TPO D-6206 This TPO product was developed for facia applications exhibiting adhesion for current automotive paint systems.Data provided by Multibase. |
|||
Tear Strength | 105 kN/m | 600 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLTHANE® 16N87 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® D16N87 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, offering adequate hardness with superior hydrolysis resistance and improved e.. |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 6 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 105 kN/m | 599 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible B6DB1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 105 kN/m | 599 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible C5D01 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 105 kN/m | 599 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible G92B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 105 kN/m | 600 pli | Injection molded parts; ASTM D624 |
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNT.. |
|||
Tear Strength | 105 kN/m | 600 pli | ASTM D624 |
Huntsman IROGRAN® A 85 D 5001 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
Tear Strength | 105 kN/m | 600 pli | ASTM D624 |
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 87 H 4615 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi.. |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM D624 |
Huntsman IROGRAN® A 95 K 4640 TPU-For Seals Introduction: IROGRAN A95K 4640 is a caprolactone-based thermoplastic polyurethane. The material has been developed for injection molding applications requiring exceptional performance in terms of c.. |
|||
Tear Strength | 105 kN/m | 600 pli | ASTM D624 |
Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Tear Strength | 105 kN/m | 599 pli | ISO 34B |
Huntsman AVALON® 85 AB Thermoplastic Polyurethane Introduction: AVALON 85 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Tear Strength | 105 kN/m | 599 pli | ISO 34B |
Huntsman AVALON® 90 AE Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
Tear Strength | 105 kN/m | 600 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® q-GUARD® 35 Insulation Jacketing Description: q-GUARD® is a thermally durable and fire-safe composite developed specifically for use with removable and reusable insulation systems. Based upon PTFE fluorocarbon resins and fibergl.. |
|||
Tear Strength | 105 kN/m | 600 pli | ASTM D624 |
Techmer ES Luriblend® TPU 40D GL10 Availability: North AmericaForms: PelletsAdditive: Graphite Powder Lubricant(10%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 6 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 105 kN/m | 599 pli | Die C; ASTM D624 |
Lubrizol Estane® 2102-80A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Tear Strength | 105 kN/m | 599 pli | Die C; ASTM D624 |
Lubrizol Estane® 2103-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Tear Strength | 105 kN/m | 599 pli | Die C; ASTM D624 |
Lubrizol Estane® 2103-84AEN Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Contains UV Stabilizer, NSF Standard 61 certifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pelletha.. |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM D624 |
Lubrizol Estane® 2355-95AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Fuel resistant, extrusion laminate coatingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Dow Chemical.Lubrizol acquired the Pellethane.. |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM D624 |
ELASTO UK Dryflex® 420501S SBS Based Material, 50D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR2202-95A Seal Grade TPU Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tear Strength | >= 105 kN/m | >= 599 pli | ISO 34 |
Austin Novel Materials Texalan® 590A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tear Strength | 105 kN/m | 599 pli | Parallel to flow; ISO 34-B |
AlphaGary Evoprene™ LF 6158 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Tear Strength | 105 kN/m | 599 pli | ASTM D624 |
BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Tear Strength | 105 kN/m | 600 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 183 PTFE Coated Fiberglass Conveyor Belting Description: General Notes on Saint Gobain SPECIALTY SERIES Belting Products:Dimensional Stability: Width rigidity as well as length stability is maintained by CHEMFAB Specialty Series belting in co.. |
|||
Tear Strength | 105 kN/m | 599 pli | Nicked; ISO 34-1B |
Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane Type: Estane® GP 52DT is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |