Material Notes:
Multi-Flex® D 6403 is a rubber modified polypropylene compound for automotive applications such as bumper-covers, step in pads, rubstrips, and airdams.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955-89
Melt Flow 3.0 g/10 min
3.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 20.7 MPa
3000 psi
ASTM D638-95
Elongation at Break >= 300 %
>= 300 %
ASTM D638-95
Flexural Modulus 0.690 GPa
100 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256-93a
Tear Strength 105 kN/m
599 pli
Die C; ASTM D-624-95