Material Notes:
Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 127 microns
5.00 mil
Carrier; Arlon SQA-TMS-003
508 microns
20.0 mil
Silicone; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 44
44
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 7.58 MPa
1100 psi
Silicone Property; Arlon SQA-TMS-008
Elongation at Break 650 %
650 %
Silicone Property; Arlon SQA-TMS-008
Tear Strength 14.5 kN/m
83.0 pli
Die B; Silicone Property; Arlon SQA-TMS-029
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 204 °C
400 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 V-0
V-0
E54153
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Post Cure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Gray
Silicone
Translucent
Carrier
Total Product Weight (oz/yd2) 18.6
Arlon SQA-TMS-025
Users viewing this material also viewed the following: