Arlon 18976XA023 Silicone Rubber/Fiberglass Laminate

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 18976XA023 Silicone Rubber/Fiberglass Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Side 1:cured silicone rubber; Substrate: 11523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
Silicone Property; Arlon SQA-TMS-024
Thickness 102 microns
4.00 mil
silicone, side 1; Arlon SQA-TMS-003
102 microns
4.00 mil
silicone, side 2; Arlon SQA-TMS-003
381 microns
15.0 mil
substrate; Arlon SQA-TMS-003
584 microns
23.0 mil
overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
Silicone Property; ASTM D2240
Tensile Strength, Ultimate 8.89 MPa
1290 psi
Silicone Property; ASTM D412
Elongation at Break 150 %
150 %
Silicone Property; ASTM D412
Adhesive Bond Strength 0.0228 MPa
3.30 psi
Arlon SQA-TMS-011
Tear Strength 14.5 kN/m
83.0 pli
Silicone, Die B; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 V-1
V-1
Electrical Properties Metric English Comments
Dielectric Strength 21.1 kV/mm
536 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Color Gray