Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 14.5 kN/m | 82.7 pli | Die C; ASTM D624 |
Teknor Apex Telcar® TL-6045 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tear Strength | 14.5 kN/m | 82.7 pli | ASTM D624 |
Teknor Apex Uniprene® UN-1141A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tear Strength | 14.5 kN/m | 82.7 pli | ASTM D624 |
Teknor Apex Uniprene® UN-7100-45 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |