Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.002943 GPa @Temperature 110 °C, Time 86400 sec |
0.4269 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories APC-120G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.006867 GPa @Temperature 1000 °C, Time 10800 sec |
0.4269 - 0.9960 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories CT-140S Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.007848 GPa @Temperature 1350 °C, Time 10800 sec |
0.4269 - 1.138 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories CT-140S Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 GPa @Temperature 110 °C, Time 86400 sec |
0.4269 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories CTC-60TD Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.006867 GPa @Temperature 110 °C, Time 86400 sec |
0.4269 - 0.9960 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HACT-165G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.006867 GPa @Temperature 1000 °C, Time 10800 sec |
0.4269 - 0.9960 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HACT-165G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.006867 GPa @Temperature 110 °C, Time 86400 sec |
0.4269 - 0.9960 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HACT-170 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.006867 GPa @Temperature 1000 °C, Time 10800 sec |
0.4269 - 0.9960 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HACT-170 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.005886 GPa @Temperature 1350 °C, Time 10800 sec |
0.4269 - 0.8537 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories INCT-160 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.005886 GPa @Temperature 1500 °C, Time 10800 sec |
0.4269 - 0.8537 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories INCT-170 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.005886 GPa @Temperature 1350 °C, Time 10800 sec |
0.4269 - 0.8537 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories PT-150 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.005886 GPa @Temperature 1350 °C, Time 10800 sec |
0.4269 - 0.8537 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.005886 GPa @Temperature 1350 °C, Time 10800 sec |
0.4269 - 0.8537 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories PT-170 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.005886 GPa @Temperature 1350 °C, Time 10800 sec |
0.4269 - 0.8537 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories PTA-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.005886 GPa @Temperature 1350 °C, Time 10800 sec |
0.4269 - 0.8537 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories PTF-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 GPa @Temperature 110 °C, Time 86400 sec |
0.4269 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories SW64 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 GPa @Temperature 1000 °C, Time 10800 sec |
0.4269 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories SW64 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.007848 GPa @Temperature 1000 °C, Time 10800 sec |
0.4269 - 1.138 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HACT-150S High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.005886 GPa @Temperature 1350 °C, Time 10800 sec |
0.4269 - 0.8537 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories PT-140 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.006867 GPa @Temperature 1350 °C, Time 10800 sec |
0.4269 - 0.9960 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories HACT-155 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.006867 GPa @Temperature 110 °C, Time 86400 sec |
0.4269 - 0.9960 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HACT-155 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.006867 GPa @Temperature 1350 °C, Time 10800 sec |
0.4269 - 0.9960 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories HACT-165 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.006867 GPa @Temperature 110 °C, Time 86400 sec |
0.4269 - 0.9960 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HACT-165 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.005886 GPa @Temperature 1350 °C, Time 10800 sec |
0.4269 - 0.8537 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories PT-150 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |