Mechanical Properties Metric English Comments
Modulus of Rupture 0.002943 - 0.007848 GPa

@Temperature 1350 °C,
Time 10800 sec
0.4269 - 1.138 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories CT-140S Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.003924 - 0.007848 GPa

@Temperature 1350 °C,
Time 10800 sec
0.5691 - 1.138 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories HACT-170 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.004905 - 0.007848 GPa

@Temperature 1500 °C,
Time 10800 sec
0.7114 - 1.138 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories PT-160 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.004905 - 0.007848 GPa

@Temperature 1500 °C,
Time 10800 sec
0.7114 - 1.138 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories PT-165 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.007848 GPa

@Temperature 1000 °C,
Time 10800 sec
0.4269 - 1.138 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HACT-150S High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).