Chosun Refractories SW64 Special High-Density Gunning Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories SW64 Special High-Density Gunning Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.74 g/cc

@Temperature 110 °C,
Time 86400 sec
0.0990 lb/in³

@Temperature 230 °F,
Time 24.0 hour
2.74 g/cc

@Temperature 1000 °C,
Time 10800 sec
0.0990 lb/in³

@Temperature 1830 °F,
Time 3.00 hour
2.78 g/cc

@Temperature 1500 °C,
Time 10800 sec
0.100 lb/in³

@Temperature 2730 °F,
Time 3.00 hour
Porosity 18.5 %

@Temperature 110 °C,
Time 86400 sec
18.5 %

@Temperature 230 °F,
Time 24.0 hour
18.5 %

@Temperature 1500 °C,
Time 10800 sec
18.5 %

@Temperature 2730 °F,
Time 3.00 hour
20 %

@Temperature 1000 °C,
Time 10800 sec
20 %

@Temperature 1830 °F,
Time 3.00 hour
Mechanical Properties Metric English Comments
Modulus of Rupture 0.002943 GPa

@Temperature 110 °C,
Time 86400 sec
0.4269 ksi

@Temperature 230 °F,
Time 24.0 hour
0.002943 GPa

@Temperature 1000 °C,
Time 10800 sec
0.4269 ksi

@Temperature 1830 °F,
Time 3.00 hour
0.013734 GPa

@Temperature 1500 °C,
Time 10800 sec
1.9920 ksi

@Temperature 2730 °F,
Time 3.00 hour
Thermal Properties Metric English Comments
Shrinkage -0.160 %

@Temperature 1000 °C,
Time 10800 sec
-0.160 %

@Temperature 1830 °F,
Time 3.00 hour
-0.0300 %

@Temperature 1500 °C,
Time 10800 sec
-0.0300 %

@Temperature 2730 °F,
Time 3.00 hour
-0.0300 %

@Temperature 110 °C,
Time 86400 sec
-0.0300 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 64 %
64 %
SiO2 3.0 %
3.0 %
Descriptive Properties Value Comments
Main Applications Blast furnace