Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Rupture = 0.002943 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.002943 GPa

@Temperature 110 °C,
Time 86400 sec
0.4269 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories APC-120G Acid-proof Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 1000 °C,
Time 10800 sec
0.4269 - 0.9960 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories CT-140S Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.007848 GPa

@Temperature 1350 °C,
Time 10800 sec
0.4269 - 1.138 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories CT-140S Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 GPa

@Temperature 110 °C,
Time 86400 sec
0.4269 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories CTC-60TD Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.4269 - 0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HACT-165G High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 1000 °C,
Time 10800 sec
0.4269 - 0.9960 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HACT-165G High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.4269 - 0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HACT-170 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 1000 °C,
Time 10800 sec
0.4269 - 0.9960 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HACT-170 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.005886 GPa

@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.8537 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories INCT-160 Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.005886 GPa

@Temperature 1500 °C,
Time 10800 sec
0.4269 - 0.8537 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories INCT-170 Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.005886 GPa

@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.8537 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories PT-150 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.005886 GPa

@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.8537 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories PT-165 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.005886 GPa

@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.8537 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories PT-170 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.005886 GPa

@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.8537 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories PTA-180 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.005886 GPa

@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.8537 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories PTF-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 GPa

@Temperature 110 °C,
Time 86400 sec
0.4269 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories SW64 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 GPa

@Temperature 1000 °C,
Time 10800 sec
0.4269 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories SW64 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.007848 GPa

@Temperature 1000 °C,
Time 10800 sec
0.4269 - 1.138 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HACT-150S High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.005886 GPa

@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.8537 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories PT-140 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.9960 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories HACT-155 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.4269 - 0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HACT-155 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.9960 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories HACT-165 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.4269 - 0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HACT-165 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.005886 GPa

@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.8537 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories PT-150 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved