Mechanical Properties Metric English Comments
Modulus of Rupture 3.37e-7 - 0.00147 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.213 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT-110N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.00147 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.213 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT-120N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.00147 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.213 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT-135N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.00147 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.213 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT135S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.00245 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.356 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories MIX-1(1:4) Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PT-150 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PT-160 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.00196 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.285 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories GUN-135L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PT-140 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PAC-160 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PT-150 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).