Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 1.44e-7 - 0.000491 GPa @Temperature 110 °C, Time 86400 sec |
0.0000209 - 0.0711 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories INCT-100S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 1.44e-7 - 0.000491 GPa @Temperature 110 °C, Time 86400 sec |
0.0000209 - 0.0711 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories INCT-110S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 2.41e-7 - 0.000491 GPa @Temperature 110 °C, Time 86400 sec |
0.0000349 - 0.0711 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories INCT-120S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 1.44e-7 - 0.000491 GPa @Temperature 110 °C, Time 86400 sec |
0.0000209 - 0.0711 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories INCT-80N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 6.74e-8 - 0.000491 GPa @Temperature 110 °C, Time 86400 sec |
0.00000977 - 0.0711 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories MIX-3 Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.37e-7 - 0.000491 GPa @Temperature 110 °C, Time 86400 sec |
0.0000489 - 0.0711 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PT-150 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.37e-7 - 0.000491 GPa @Temperature 110 °C, Time 86400 sec |
0.0000489 - 0.0711 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PT-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.37e-7 - 0.000491 GPa @Temperature 110 °C, Time 86400 sec |
0.0000489 - 0.0711 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PT-140 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.37e-7 - 0.000491 GPa @Temperature 110 °C, Time 86400 sec |
0.0000489 - 0.0711 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PAC-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.37e-7 - 0.000491 GPa @Temperature 110 °C, Time 86400 sec |
0.0000489 - 0.0711 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PT-150 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |