Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 2.41e-7 - 0.00147 GPa @Temperature 110 °C, Time 86400 sec |
0.0000349 - 0.213 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories GUN-80L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 2.41e-7 - 0.00147 GPa @Temperature 110 °C, Time 86400 sec |
0.0000349 - 0.213 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories INCT-100N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.37e-7 - 0.00147 GPa @Temperature 110 °C, Time 86400 sec |
0.0000489 - 0.213 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories INCT-110N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.37e-7 - 0.00147 GPa @Temperature 110 °C, Time 86400 sec |
0.0000489 - 0.213 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories INCT-120N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.37e-7 - 0.00147 GPa @Temperature 110 °C, Time 86400 sec |
0.0000489 - 0.213 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories INCT-135N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.37e-7 - 0.00147 GPa @Temperature 110 °C, Time 86400 sec |
0.0000489 - 0.213 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories INCT135S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 4.33e-7 - 0.00147 GPa @Temperature 110 °C, Time 86400 sec |
0.0000628 - 0.213 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories INCT-140 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 4.33e-7 - 0.00147 GPa @Temperature 110 °C, Time 86400 sec |
0.0000628 - 0.213 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories INCT-160 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |