Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 3.37e-7 - 0.00245 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.356 ksi

@Temperature 230 °F,
Time 24.0 hour
0.000981 - 0.0024525 GPa

@Temperature 1000 °C,
Time 10800 sec
0.142 - 0.35571 ksi

@Temperature 1830 °F,
Time 3.00 hour
Compressive Strength 4.90 - 14.7 MPa

@Temperature 1000 °C,
Time 10800 sec
711 - 2130 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
9.81 - 19.6 MPa

@Temperature 110 °C,
Time 86400 sec
1420 - 2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.233 - 0.4653 W/m-K

@Temperature 540 °C
1.61 - 3.224 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.349 - 0.6979 W/m-K

@Temperature 800 °C
2.42 - 4.836 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 1100 °C
2010 °F
limited
Shrinkage -1.00 - -0.700 %

@Temperature 1000 °C,
Time 10800 sec
-1.00 - -0.700 %

@Temperature 1830 °F,
Time 3.00 hour
0.00 %

@Temperature 110 °C,
Time 86400 sec
0.00 %

@Temperature 230 °F,
Time 24.0 hour
Descriptive Properties Value Comments
Installation Method Gunning, Casting(UOP)
Main Applications Petrochemical plant Heater, Boiler
Material Required for Estimating (kg/?) 1,200-1,500
Water Required for Casting(%) 35