Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 3.37e-7 - 0.00196 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.285 ksi

@Temperature 230 °F,
Time 24.0 hour
0.000981 - 0.001962 GPa

@Temperature 1000 °C,
Time 10800 sec
0.142 - 0.2846 ksi

@Temperature 1830 °F,
Time 3.00 hour
Compressive Strength 2.45 - 4.41 MPa

@Temperature 1000 °C,
Time 10800 sec
356 - 640 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
5.69 - 5.88 MPa

@Temperature 110 °C,
Time 86400 sec
825 - 853 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.4653 W/m-K

@Temperature 260 °C
3.224 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.48852 W/m-K

@Temperature 540 °C
3.3849 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.55831 W/m-K

@Temperature 800 °C
3.8684 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 1350 °C
2460 °F
limited
Shrinkage -0.400 %

@Temperature 1000 °C,
Time 10800 sec
-0.400 %

@Temperature 1830 °F,
Time 3.00 hour
-0.100 %

@Temperature 110 °C,
Time 86400 sec
-0.100 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 37 %
37 %
SiO2 41 %
41 %
Descriptive Properties Value Comments
Installation Method Gunning
Main Applications Fireproof insulating Part
Material Required for Estimating (kg/?) 1,450
Water Required for Casting(%) Nozzle Mixing