Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 3.37e-7 - 0.00245 GPa @Temperature 110 °C, Time 86400 sec |
0.0000489 - 0.356 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories MIX-1(1:4) Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |