Polymer Property : Puncture Energy = 2.21 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 1.60 - 3.00 J

@Temperature -30.0 - -30.0 °C
1.18 - 2.21 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 2.65 J Grade Count:2
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Puncture Energy 3.00 - 3.00 J

@Temperature -30.0 - -30.0 °C
2.21 - 2.21 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 2.65 J Grade Count:2
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Puncture Energy 3.00 - 3.00 J

@Load <=74.2 kg
2.21 - 2.21 ft-lb

@Load <=164 lb
Average value: 2.65 J Grade Count:2
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..