Mechanical Properties Metric English Comments
Flexural Modulus 3.45 - 9.65 GPa
500 - 1400 ksi
Average value: 6.85 GPa Grade Count:31
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Flexural Modulus 2.06 - 9.65 GPa
299 - 1400 ksi
Average value: 2.75 GPa Grade Count:49
Overview of materials for Polyphenylene Ether, Heat Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu..
Flexural Modulus 3.33 - 9.65 GPa
484 - 1400 ksi
Average value: 7.20 GPa Grade Count:89
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Flexural Modulus 2.60 - 9.65 GPa
377 - 1400 ksi
Average value: 3.97 GPa Grade Count:12
Overview of materials for Nylon 66, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate..
Flexural Modulus 1.80 - 9.65 GPa
261 - 1400 ksi
Average value: 5.10 GPa Grade Count:34
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
Flexural Modulus 8.27 - 9.65 GPa
1200 - 1400 ksi
Bulk Molding Compounds BMC T14 General Purpose Molding Compound
BMC T14 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T14 is well suited for injection, transfer or compression molding of intricate parts. Typica..
Flexural Modulus 8.27 - 9.65 GPa
1200 - 1400 ksi
Bulk Molding Compounds BMC T9 General Purpose Molding Compound
BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9..
Flexural Modulus 8.27 - 9.65 GPa
1200 - 1400 ksi
Bulk Molding Compounds BMC A50-MS General Purpose Molding Compound
BMC A50-MS is a medium strength, high appearance, general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A50-MS is well suited for injection, transfer or compres..
Flexural Modulus 2.96 - 9.65 GPa
430 - 1400 ksi
Average value: 7.58 GPa Grade Count:11
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma..
Flexural Modulus 1.90 - 9.65 GPa
276 - 1400 ksi
Average value: 4.72 GPa Grade Count:26
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Flexural Modulus 8.27 - 9.65 GPa
1200 - 1400 ksi
ASTM D790
Premix Premi-Glas® 1200H-24 Polyester SMC  (discontinued **)
Premi-Glas® 1200H-24 is a 24% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where arc resistance and dielectric strength are required and UL 94 HB flame recogni..
Flexural Modulus 8.27 - 9.65 GPa
1200 - 1400 ksi
ASTM D790
Premix Premi-Glas® 1200-24 Polyester SMC  (discontinued **)
Premi-Glas® 1200-24 is a 24% fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck - Bus body panels and Marine cowls parts where smooth, flat, ripple free surfa..
Flexural Modulus 8.27 - 9.65 GPa
1200 - 1400 ksi
ASTM D790
Premix Premi-Glas® 1200-28 Polyester SMC  (discontinued **)
Premi-Glas® 1200-28 series is a low profile, 28 % glass reinforced polyester Sheet Molding Compound designed for recreational vehicle body panels applications that require excellent flexibility and..