Mechanical Properties Metric English Comments
Flexural Modulus 3.33 - 9.65 GPa
484 - 1400 ksi
Average value: 7.20 GPa Grade Count:89
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Flexural Modulus 3.33 GPa
484 ksi
ASTM D790
Lendell Parapet EH-1000 PMMA, Extrusion
Flexural Modulus 3.33 GPa

@Thickness 3.20 mm
484 ksi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance
Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG ..
Flexural Modulus 3.33 GPa
484 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® NH-1101 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Flexural Modulus 3.33 GPa
484 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® NH-1101 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Flexural Modulus 3.34 GPa
484 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp TX88477 PU
LNP* Thermocomp* TX88447 is a compound based on Polyurethane resin containing proprietary fillers.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 3.33 GPa
484 ksi
ASTM D790
Samyang Trirex® 3025GRU30 Polycarbonate, 30% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electr..