Bulk Molding Compounds BMC T9 General Purpose Molding Compound

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC T9 General Purpose Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9 can be compression, transfer or injection molded. Other applications re bobbins and electrical connectors.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 1.96 - 2.16 g/cc
0.0708 - 0.0780 lb/in³
Molded
Linear Mold Shrinkage 0.0020 - 0.0038 cm/cm
0.0020 - 0.0038 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 30 - 50
30 - 50
Tensile Strength 48.3 - 62.1 MPa
7000 - 9000 psi
Flexural Strength 110 - 138 MPa
16000 - 20000 psi
Flexural Modulus 8.27 - 9.65 GPa
1200 - 1400 ksi
Compressive Strength 131 - 159 MPa
19000 - 23000 psi
Izod Impact, Notched 2.67 - 3.74 J/cm
5.00 - 7.00 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength 13.8 - 15.7 kV/mm
350 - 400 kV/in
short time
Arc Resistance >= 180 sec
>= 180 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Processing Temperature 138 - 166 °C
280 - 330 °F