Mechanical Properties Metric English Comments
Flexural Modulus 0.600 - 4.30 GPa

@Temperature -40.0 - 90.0 °C
87.0 - 624 ksi

@Temperature -40.0 - 194 °F
Average value: 1.92 GPa Grade Count:4
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Flexural Modulus 0.400 - 4.30 GPa

@Temperature -40.0 - 80.0 °C
58.0 - 624 ksi

@Temperature -40.0 - 176 °F
Average value: 2.14 GPa Grade Count:2
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Flexural Modulus 1.20 - 4.30 GPa
174 - 624 ksi
Average value: 2.43 GPa Grade Count:106
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..