Mechanical Properties Metric English Comments
Flexural Modulus 4.65 GPa
675 ksi
Tangent; ASTM D790
RheTech Products F43-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Fan shroudsDip trayFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 4.65 GPa
675 ksi
Tangent; ASTM D790
RheTech Products GC35P200-01UV 35% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, General Purpose Black
Applications: BracketsStructural componentsHeadlamp housingsWindow frameInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 4.65 GPa
674 ksi
ASTM D790
PolyOne Nymax™ GBF 1200 23 HS BLACK 18 Polyamide 66 (Nylon 66)
Information provided by PolyOne
Flexural Modulus 4.65 GPa
674 ksi
ASTM D790
Nylene® PA6/6 Glass Filled 5113 HS Nylon 6/6
13% Glass Filler; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Flexural Modulus 4.65 GPa
675 ksi
ASTM D790
Oxford Polymers 15GF-V0 15% Glass Fiber Reinforced Polybutylene Terephthalate (PBT), Flame Resistant
15% Glass Fiber Reinforced Polybutylene Terephthalate (PBT), Flame ResistantInformation provided by Oxford Polymers.
Flexural Modulus 4.65 GPa
675 ksi
ASTM D790
Oxford Polymers PBT 15GF-V0 UL Listed Polybutylene Terephthalate (PBT)
UL Listed Polybutylene Terephthalate (PBT)Information provided by Oxford Polymers.
Flexural Modulus 4.65 GPa
674 ksi
ASTM D790
PTS Trimid® N66-G13 13% Glass Fiber Reinforced Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 4.65 GPa
674 ksi
ASTM D790
Penn Fibre Pennite® 4512 Nylon 6, 12% Glass Fiber Reinforced (PA6)
PENNITE® 4512 is a 12% glass fiber reinforced, black pigmented, thermally modified, type 6 nylon, available in sheets and rolls for high performance thermoforming and fabrication applications. PENN..
Flexural Modulus 4.65 GPa
674 ksi
ASTM D790
LNP Thermocomp® JF-1004 EM M BK905 Polyethersulfone, Milled Glass Fiber  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
Flexural Modulus 4.65 GPa
675 ksi
ASTM D790
Ravago Manufacturing Americas Hylon® N1020MHL Nylon 6/6  (discontinued **)
Available in North America Filler: Mineral, 20% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedForm: Pellets Processing Method: Injection MoldingIn..
Flexural Modulus 4.65 GPa
675 ksi
ASTM D790
Techmer ES HiFill® TPX-PBT-98010 BN069
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityAppearance: Light BeigeProcessing Method: Injection MoldingInformation provided by TP C..
Flexural Modulus 4.65 GPa
674 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOTUF PX07437 PA 6
Compound based on Nylon 6 resin containing glass fiber and impact modifier.
Flexural Modulus 4.65 GPa
675 ksi
ASTM D790
Teknor Apex Chemlon® 113 GH Nylon 66, 13% Short Glass Fiber Reinforced
Features: Good creep Resistance; Good stiffness; Good dimensional stability; High strength; Heat stabilized Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS..
Flexural Modulus 4.65 GPa
675 ksi
ASTM D790
Teknor Apex Synres® PP G30 19 Polypropylene, Glass Reinforced
Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many ..
Flexural Modulus 4.65 GPa
675 ksi
ASTM D790
Chase Plastics CP Pryme® NN113GL (DAM) Nylon 66, 13% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Flexural Modulus 4.65 GPa
675 ksi
ASTM D790
Chase Plastics CP Pryme® NN213GL (DAM) Nylon 66, 13% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Flexural Modulus 4.65 GPa
675 ksi
ASTM D790
Ecomass® 1080ZD92 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade
High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing..
Flexural Modulus 4.65 GPa
675 ksi
ASTM D790
Ecomass® 1080ZD93 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade
High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing..
Flexural Modulus 4.65 GPa
674 ksi
ASTM Test
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Dry)
Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the..
Flexural Modulus 4.65 GPa
675 ksi
ASTM D-790
Axiall Tuf-Stif 2804 Rigid PVC, Extrusion
Georgia Gulf Tuf-Stif 2804 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit..