Material Notes:
High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiation shielding applicationsInformation provided by Technical Polymers.
Physical Properties Metric English Comments
Specific Gravity 8.00 g/cc
8.00 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 37.9 MPa
5500 psi
ASTM D638
Elongation at Break 4.1 %
4.1 %
ASTM D638
Tensile Modulus 6.58 GPa
955 ksi
ASTM D638
Flexural Strength 49.6 MPa
7200 psi
ASTM D790
Flexural Modulus 4.65 GPa
675 ksi
ASTM D790
Izod Impact, Notched 1.55 J/cm
2.90 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
225 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.21 ohm
0.21 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 204 - 254 °C
400 - 490 °F
Mold Temperature 57.2 - 82.2 °C
135 - 180 °F
Drying Temperature 73.9 °C
165 °F
Dry Time 4 hour
4 hour
Users viewing this material also viewed the following: