Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.65 GPa | 675 ksi | Tangent; ASTM D790 |
RheTech Products F43-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Fan shroudsDip trayFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 4.65 GPa | 675 ksi | Tangent; ASTM D790 |
RheTech Products GC35P200-01UV 35% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, General Purpose Black Applications: BracketsStructural componentsHeadlamp housingsWindow frameInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 4.65 GPa | 675 ksi | ASTM D790 |
Oxford Polymers 15GF-V0 15% Glass Fiber Reinforced Polybutylene Terephthalate (PBT), Flame Resistant 15% Glass Fiber Reinforced Polybutylene Terephthalate (PBT), Flame ResistantInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 4.65 GPa | 675 ksi | ASTM D790 |
Oxford Polymers PBT 15GF-V0 UL Listed Polybutylene Terephthalate (PBT) UL Listed Polybutylene Terephthalate (PBT)Information provided by Oxford Polymers. |
|||
Flexural Modulus | 4.65 GPa | 675 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1020MHL Nylon 6/6
(discontinued **) Available in North America Filler: Mineral, 20% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedForm: Pellets Processing Method: Injection MoldingIn.. |
|||
Flexural Modulus | 4.65 GPa | 675 ksi | ASTM D790 |
Techmer ES HiFill® TPX-PBT-98010 BN069 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityAppearance: Light BeigeProcessing Method: Injection MoldingInformation provided by TP C.. |
|||
Flexural Modulus | 4.65 GPa | 675 ksi | ASTM D790 |
Teknor Apex Chemlon® 113 GH Nylon 66, 13% Short Glass Fiber Reinforced Features: Good creep Resistance; Good stiffness; Good dimensional stability; High strength; Heat stabilized Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS.. |
|||
Flexural Modulus | 4.65 GPa | 675 ksi | ASTM D790 |
Teknor Apex Synres® PP G30 19 Polypropylene, Glass Reinforced Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many .. |
|||
Flexural Modulus | 4.65 GPa | 675 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN113GL (DAM) Nylon 66, 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 4.65 GPa | 675 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN213GL (DAM) Nylon 66, 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 4.65 GPa | 675 ksi | ASTM D790 |
Ecomass® 1080ZD92 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing.. |
|||
Flexural Modulus | 4.65 GPa | 675 ksi | ASTM D790 |
Ecomass® 1080ZD93 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing.. |
|||
Flexural Modulus | 4.65 GPa | 675 ksi | ASTM D-790 |
Axiall Tuf-Stif 2804 Rigid PVC, Extrusion Georgia Gulf Tuf-Stif 2804 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit.. |