Material Notes:
Compound based on Nylon 6 resin containing glass fiber and impact modifier.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm

@Time 86400 sec
0.0030 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 - 0.0090 cm/cm

@Time 86400 sec
0.0080 - 0.0090 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 94.0 MPa
13600 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 97.0 MPa
14100 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 4.5 %
4.5 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 3.4 %
3.4 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 5.20 GPa
754 ksi
50 mm/min; ASTM D638
Flexural Strength 150 MPa
21800 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 4.65 GPa
674 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 2.00 J/cm
3.75 ft-lb/in
ASTM D256
Izod Impact, Unnotched 10.7 J/cm
20.0 ft-lb/in
ASTM D4812
Dart Drop, Total Energy 5.00 J
3.69 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
25.0 J

@Temperature 23.0 °C
18.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 190 °C

@Thickness 3.20 mm
374 °F

@Thickness 0.126 in
unannealed; ASTM D648