Mechanical Properties Metric English Comments
Flexural Modulus 1.89 GPa
274 ksi
1.3 mm/min, 50 mm span; ASTM D790
Ovation Polymers Opnyl OP66UT105 Nylon 66
Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All..
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified
General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples...
Flexural Modulus 1.89 GPa

@Thickness 6.40 mm
274 ksi

@Thickness 0.252 in
ASTM D 790
SABIC Innovative Plastics Lexan® FL3000 PC
Structural foam: 10% weight reduction at 0.250" wall with non-brominated and non-chlorinated FR systems. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supp..
Flexural Modulus 1.89 GPa

@Thickness 6.40 mm
274 ksi

@Thickness 0.252 in
ASTM D 790
SABIC Innovative Plastics Lexan® FL3000 PC (Asia Pacific)
Structural foam: 10% weight reduction at 0.250" wall. ECO-conforming. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supplied by SABIC-IP for the Asia Paci..
Flexural Modulus 1.89 - 2.96 GPa
274 - 430 ksi
Average value: 2.47 GPa Grade Count:58
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated.
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific)
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 1.89 GPa
274 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific)
Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 1.89 GPa
274 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East)
Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 1.89 GPa
274 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-LOY 9X07438 ASA+PC
LNP* STAT-LOY* 9X07438 is a compound based on Polycarbonate/ASA containing Proprietary Filler(s). Added features of this grade include: Antistatic, Colorable, Weatherable.
Flexural Modulus 1.89 GPa
274 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-LOY W3000XXJ PBT
LNP* STAT-LOY* W3000XXJ is a compound based on PBT. Added features of this grade include: Anti-Stat, Colorable, Healthcare
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1245U CaCO3 Filled UV Stable Copolymer Polypropylene
DescriptionPolyfort® FPP 1245U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1245U CaCO3 Filled UV Stable Copolymer Polypropylene
DescriptionPolyfort® FPP 1245U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1245U CaCO3 Filled UV Stable Copolymer Polypropylene
DescriptionPolyfort® FPP 1245U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1245U CaCO3 Filled UV Stable Copolymer Polypropylene
DescriptionPolyfort® FPP 1245U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1245U CaCO3 Filled UV Stable Copolymer Polypropylene
DescriptionPolyfort® FPP 1245U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 1.89 GPa
274 ksi
ISO 178
ExxonMobil Exxtral™ BMU 233 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact, good dimensional stability and good UV resistance.Availability..
Flexural Modulus 1.89 GPa
274 ksi
ASTM Test
BASF Ultramid® 8350 HS BK-102 PA6 (Dry)
Ultramid 8350 HS BK-102 is a type 6, black pigmented, impact modified graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a..
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 1.89 GPa
274 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1245U CaCO3 Filled UV Stable Copolymer Polypropylene
DescriptionPolyfort® FPP 1245U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman.