Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ovation Polymers Opnyl OP66UT105 Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Ovation Polymers
Trade Name Opnyl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Opnyl OP66UT105 Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Linear Mold Shrinkage 0.0080 - 0.011 cm/cm

@Thickness 3.17 mm
0.0080 - 0.011 in/in

@Thickness 0.125 in
Linear Mold Shrinkage, Transverse 0.0145 - 0.016 cm/cm

@Thickness 3.17 mm
0.0145 - 0.016 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
50 mm/min; ASTM D638
Elongation at Break 25 %
25 %
50 mm/min; ASTM D638
Tensile Modulus 1.80 GPa
261 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 70.0 MPa
10200 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1.89 GPa
274 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 5.50 J/cm
10.3 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
@ 15°C/min; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C

@Thickness 3.20 mm
147 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved